The toy surface saliva resistance soaking test evaluates whether coatings, paints, prints, and colorants on toys can withstand prolonged contact with saliva without bleeding, fading, or transferring harmful substances into a child's mouth. This test is essential for toys intended for children under 36 months and any mouthable toy, supporting compliance with standards such as DIN 53160-1 and the requirements of the EU Toy Safety Directive. This article explains the technical principle, sample types, test items, methods, and typical applications of the saliva resistance soaking test.
Technical Overview
Infants and toddlers routinely mouth, suck, and chew their toys. During this behavior, toy surfaces remain in continuous contact with saliva, which is a warm, mildly acidic-to-neutral electrolyte solution capable of dissolving or swelling certain colorants, binders, and coating films. If a surface coating, printed pattern, or dyed material is not sufficiently resistant to saliva, pigments and dyes may bleed out of the substrate and be swallowed by the child.
The toy surface saliva resistance soaking test, also known as the colorfastness-to-artificial-saliva test, simulates this mouthing scenario under controlled laboratory conditions. Test specimens are exposed to artificial saliva by immersion or contact methods, and the degree of color bleeding, staining of adjacent absorbent material, and change in surface appearance is assessed after a defined exposure period. The test is widely applied alongside chemical migration tests such as EN 71-3 to demonstrate that mouthable toy surfaces are safe under realistic and reasonably foreseeable use.
Key reference frameworks include DIN 53160-1 for colorfastness of articles of common use in artificial saliva, DIN 53160-2 for artificial sweat, EN 71-3 for migration of certain elements, ISO 105-A02 and ISO 105-A03 grey scales for evaluation, and relevant national toy and infant-textile requirements under the GB standards family. ASTM F963 and EN 71 series provide the broader toy safety context in which saliva contact is considered.
Testing Samples
Sample selection should focus on all surfaces that a child can realistically bring into the mouth. Each distinct material, color, and coating type should be treated as a separate test specimen.
Painted and Coated Toy Surfaces
Wooden toys, metal toys, and some plastic toys finished with solvent-borne, water-borne, or UV-cured paints and lacquers. These coatings are the most common source of saliva bleeding failures, particularly when pigments are poorly bound or under-cured.
Printed Surfaces and Transfers
Pad-printed, screen-printed, heat-transfer, and water-transfer decorations applied to plastic housings, plush toy eyes and labels, and paper or cardboard components. Inks and transfer films are evaluated for bleeding when soaked in artificial saliva.
Textile and Plush Toy Components
Dyed and printed fabrics on stuffed animals, dolls, soft books, and textile accessories. For infant textiles, national requirements such as those in the GB standards system explicitly require colorfastness to saliva for the highest safety category.
Plastic and Rubber Components
Colored thermoplastics, elastomers, teethers, and rubber parts where colorants may be incorporated into the polymer matrix or applied as surface lacquers. Migration-prone masterbatches are a known risk area.
Laminates, Stickers, and Multilayer Materials
Decorative foils, sticker appliques, and coated paperboard used in interactive books and packaging-integrated toys, where adhesive and coating layers can soften or release colorants on soaking.
Testing Items
The core scope of the saliva resistance soaking test covers the following items:
- Colorfastness of the toy surface to artificial saliva, rated on the grey scale
- Degree of color bleeding or staining transferred to an adjacent absorbent medium such as filter paper or multifiber fabric
- Color change of the specimen itself after saliva exposure, including fading, blushing, or discoloration
- Coating and surface integrity after soaking, including softening, swelling, blistering, cracking, or flaking
- Visual evidence of dye or pigment migration from colored areas to uncolored areas of the same article
- Optional complementary assessment of migration of certain elements in accordance with EN 71-3 where regulatory verification is required
Testing Methods
Test Principle
A test specimen is exposed to a standardized artificial saliva solution under defined temperature and time conditions, either by full immersion of the component or by contact of saliva-wetted absorbent material against the decorated surface under load. After exposure, the staining of the adjacent medium and the change in specimen appearance are evaluated against calibrated grey scales, and the surface condition is inspected for deterioration.
Artificial Saliva Preparation
The test reagent is an aqueous electrolyte solution formulated to simulate the ionic composition and pH of natural saliva, typically based on the formulation specified in DIN 53160-1. The solution commonly contains sodium chloride, potassium chloride, calcium chloride, and sodium bicarbonate, with or without mucin depending on the referenced protocol, adjusted to a pH of approximately 6.8. Distilled or deionized water of at least grade 2 purity per ISO 3696 is used for preparation, and the solution is freshly prepared for each test series.
Specimen Preparation and Soaking Procedure
A typical laboratory procedure proceeds as follows:
- Cut or select representative specimens containing all decorative colors and coating types present on the finished toy; a full component may be tested where cutting is not appropriate
- Condition the specimens at standard laboratory atmosphere before testing to ensure reproducible results
- Immerse the specimens completely in artificial saliva at 37 ± 2 °C, simulating mouth temperature, ensuring a sufficient liquor-to-specimen ratio so the specimen is freely wetted
- Maintain the exposure for the duration specified by the applicable protocol, commonly in the range of 30 minutes to 2 hours; for contact-method testing per DIN 53160-1, saliva-wetted filter paper is pressed against the surface under a defined load for the specified time
- For staining assessment, place a strip of white filter paper or multifiber adjacent fabric in intimate contact with the colored surface during the exposure period
- After exposure, remove the specimen, rinse lightly if required by the protocol, and allow the specimen and the adjacent medium to dry naturally at room temperature without rubbing
Evaluation and Pass Criteria
The dried adjacent medium is rated for staining using the grey scale for staining in accordance with ISO 105-A03, and the specimen is rated for color change using the grey scale for color change in accordance with ISO 105-A02. Both scales run from grade 1, severe staining or change, to grade 5, negligible or no visible effect. The specimen surface is additionally inspected visually for softening, swelling, tackiness, cracking, or loss of adhesion of the coating.
Typical acceptance criteria applied by buyers and market surveillance authorities require a staining grade of at least 4, and in stricter specifications 4-5, together with no visible bleeding of color and no coating deterioration that could release fragments. For infant textile products, applicable national standards under the GB framework commonly require colorfastness to saliva of grade 4 or higher for the highest safety category. Test reports issued by accredited third-party laboratories should document the specimen description, the referenced method, exposure conditions, the grey scale ratings for both staining and color change, and photographic evidence where relevant.
Applications
The saliva resistance soaking test is applied across the full toy supply chain, from design validation to market surveillance:
- Compliance verification for toys intended for children under 36 months, where mouthing is an expected behavior under the EU Toy Safety Directive and equivalent national regulations
- Safety assessment of mouthable toy categories including teethers, rattles, baby dolls, soft toys, bath toys, and musical toys with suckable protrusions
- Quality control during incoming material inspection, production batches, and pre-shipment sampling to detect under-cured coatings, substandard inks, and unstable pigments before products reach the market
- Coating and ink supplier qualification programs comparing candidate colorants, binders, and finishing systems for saliva fastness performance
- Supporting documentation for CE marking under EN 71 series requirements, ASTM F963 conformity in North America, and GB 6675 conformity in China, where saliva contact is part of the foreseeable-use risk assessment
- Failure analysis and root-cause investigation when color bleeding complaints, staining incidents, or regulatory non-conformities are reported for mouthing-aged products
FAQ
Why is saliva resistance testing required for toys?
Young children mouth toys for extended periods, and saliva can dissolve or swell coatings, inks, and dyes that appear stable under dry conditions. The test verifies that no visible color bleeding or coating deterioration occurs during mouthing, which is a fundamental safety requirement for toys intended for children under 36 months and for any toy with mouthable components.
Which standard governs the test?
The primary method is DIN 53160-1, which specifies the determination of colorfastness of articles of common use in artificial saliva, including the reagent formulation, exposure conditions, and grey scale evaluation. Evaluation scales are defined in ISO 105-A02 and ISO 105-A03, and the test is commonly performed together with EN 71-3 element migration analysis as part of a complete toy safety assessment.
What results are considered a pass?
A passing result is typically a staining grade of at least 4 on the grey scale, no visible bleeding of color from the toy surface, and no softening, flaking, or other deterioration of the coating after soaking. Stricter buyer specifications may require grade 4-5. Requirements for infant textiles under national GB standards similarly specify grade 4 or above for colorfastness to saliva.
How is the saliva test different from the sweat test?
The two tests use different artificial body fluids and simulate different exposure routes. The saliva test per DIN 53160-1 addresses mouthing and ingestion risk, while the sweat test per DIN 53160-2 uses artificial perspiration and addresses prolonged skin contact. Toys worn against the skin, such as costume items, are often assessed against both.
What sample size and turnaround are typical?
Laboratories generally require one or more complete components covering every decorative color and coating type, and additional spare units if retesting is anticipated. The exposure and drying stages are short, so testing at accredited third-party laboratories is typically completed within a few working days once specimens are received.
Can the saliva test replace chemical migration testing?
No. The saliva soaking test is a fastness and physical-stability assessment that detects visible color transfer and coating breakdown. It complements, but does not replace, quantitative chemical analysis such as EN 71-3 element migration, since colorless or low-level chemical migration cannot be detected by visual grey scale rating alone. A complete conformity program includes both.
Why Choose ZKGX?
- State-of-the-art analytical equipment